Title: Dynamic load testing for the Constitución de 1812 cable-stayed Bridge over the Cadiz Bay

Author(s): Puchol de Celis, V.; Ríos de Francisco, J. de los; Castro Rubal, J. L.

Publication: ACHE

Volume: 67

Issue: 278

Appears on pages(s): 191 - 193

Keywords: Cable-stayed bridge, Dynamic test, Damping, Fusible

DOI:

Date: 1/3/2016

Abstract:
In order to comply with the requirements of the Spanish codes for bridges with a span over 60 m, a dynamic loading test was carried out to accurately obtain the dynamic parameters of the structure.