Title: On the limit analysis static method of reinforced concrete plates

Author(s): Quintas Ripoll, V.

Publication: ACHE

Volume: 45

Issue: 190

Appears on pages(s): 15-Sep

Keywords:

DOI:

Date: 1/1/1994

Abstract:
In this paper, a study of limit analysis of reinforced concrete plates is done. The equivalence between static and cinematic methods ios explained. A criterium based on on the boundary conditions is given to define if a yield-line configuration is a correct one.