Title: Cracking reinforced concrete beams under flexural loads: Time evolution

Author(s): Benlloch, J.; Barbera, E.; Perepérez Ventura, B.; Fran, J.M.; González Isabel, G.

Publication: ACHE

Volume: 42

Issue: 178

Appears on pages(s): 31 - 35

Keywords:

DOI:

Date: 1/1/1991

Abstract:
The results of an study on spacing of cracks and crackwidth of 10 reinforced concrete beams, are shown. Her time-behaviour is analyzed and the influence of compression reinforcement ratio are related to the current prediction formulae.