Concrete Q&A: ACI 318M-14 versus ACI 318-14—Eq. 18.10.4.1 and Fig. R18.7.5.2

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Q&A: ACI 318M-14 versus ACI 318-14—Eq. 18.10.4.1 and Fig. R18.7.5.2

Author(s):

Publication: Concrete International

Volume: 39

Issue: 2

Appears on pages(s): 80

Keywords:

DOI:

Date: 2/1/2017

Abstract:
Equation (18.10.4.1) of ACI 318M-141 looks the same as Eq. (18.10.4.1) in ACI 318-14.2 Why do the values assigned to the coefficient αc vary by a factor of 12 between the two versions of the code?




  