Title: From Trash to Treasure

Author(s): Christopher C. Ferraro, John P. Power, Justin Roessler, Jerry Paris, and Timothy G. Townsend

Publication: Concrete International

Volume: 38

Issue: 11

Appears on pages(s): 46-51

Keywords: mixture, placement, testing, strength

DOI:

Date: 11/1/2016

Abstract:
A pilot two-lane pavement project was recently completed in Florida using bottom ash as a partial aggregate replacement in portland cement concrete. The ash was produced at a waste-to-energy (WTE) facility in Florida. Construction of the roadway demonstrated that incorporation of WTE bottom ash did not adversely affect the workability or placement of the concrete.




  