Title: Reinforced Concrete in Motion

Author(s): Mete A. Sozen

Publication: Special Publication

Volume: 311

Issue:

Appears on pages(s): 1-16

Keywords: deflection limit, ductility, flexural strength, load-deflection relationship, moment-curvature

Date: 9/1/2016

Abstract:
Among his many achievements, Professor Wight’s observation and explanation of the irrelevance of the linear-plastic model for the moment-curvature relationship of a structural element subjected to a moment gradient (rather than constant moment) along its span stands out as one of his best contributions and one that will stand the test of time.