Title: Evolution of the ACI 562 Code––Part 3

Author(s): Gene R. Stevens and Keith Kesner

Publication: Concrete International

Volume: 38

Issue: 4

Appears on pages(s): 63-69

Keywords: strengthening, deterioration, construction, capacity

DOI: 10.14359/51688900

Date: 4/1/2016

Abstract:
An updated version of the ACI 562 Code has been reviewed by the ACI Technical Activities Committee, and ACI Committee 562 is now addressing public comments. This article is the third of a series of articles intended to explain the rationale behind some of the upcoming changes in the ACI 562 Code. It continues a discussion on assessment criteria and presents a framework within the new Code that explains when the licensed design professional must consider strengthening of a member that experiences less than substantial structural damage.

Related References:

1. “2015 IEBC Code and Commentary,” International Code Council, Washington, DC, 2015.

2. “ACI Concrete Terminology (ACI CT-13),” American Concrete Institute, Farmington Hills, MI, 2013, 74 pp.

3. “Minimum Design Loads for Buildings and Other Structures (ASCE/SEI 7-10),” American Society of Civil Engineers, Reston, VA, 2010, 608 pp.

4. Galambos, T.V.; Ellingwood, B.R.; MacGregor, J.G.; and Cornell, C.A., “Probability Based Load Criteria: Assessment of Current Design Practice,” Journal of the Structural Division, ASCE, V. 108, No. 5, May 1982, pp. 959-977.

5. Galambos, T.V.; Ellingwood, B.R; MacGregor, J.G.; and Cornell, C.A., “Probability Based Load Criteria: Load Factors and Load Combinations,” Journal of the Structural Division, ASCE, V. 108, No. 5, May 1982, pp. 978-997.

6. “ANSI A58.1-1982: Design Loads for Buildings and Other Structures,” American National Standards Institute, New York, NY, 1982, 103 pp.

7. Ellingwood, B.R., and Ang, A.H.-S., “A Probabilistic Study of Safety Criteria for Design,” SRS-387, University of Illinois at Urbana-Champaign, Champaign, IL, 1972, 195 pp.

8. “Seismic Evaluation and Retrofit of Existing Buildings (ASCE/SEI 41-13),” American Society for Civil Engineers, Reston, VA, 2014, 35 pp.

9. “Uniform Building Code,” 1979 Edition, International Conference of Building Officials, Whittier, CA, 1979, 734 pp.

10. “Manual of Steel Construction: Load and Resistance Factor Design,” first edition, American Institute of Steel Construction, Chicago, IL, 1986, 400 pp.

11. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.