364.10T-14: Rehabilitation of Structure with Reinforcement Section Loss (TechNote)

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: 364.10T-14: Rehabilitation of Structure with Reinforcement Section Loss (TechNote)

Author(s): ACI Committee 364

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 4

Keywords: concrete cover; corrosion; load-carrying capacity; rehabilitation; reinforcement; repair.

Date: 7/1/2014

Abstract:

Note: 364.10T-14 is only available in PDF format.

Integrity of reinforcement is fundamental to the strength, ductility, and safety of reinforced concrete structures. Determining the necessity of additional or replacement reinforcement is a primary concern in rehabilitation projects containing corrosion of reinforcing steel.