Title: Photocatalytic Efficiency of Cement-Based Materials: Demonstration of Proposed Test Method

Author(s): Amal R. Jayapalan, Bo Yeon Lee, Eva M. Land, Michael H. Bergin, and Kimberly E. Kurtis

Publication: Materials Journal

Volume: 112

Issue: 2

Appears on pages(s): 219-228

Keywords: characterization; photocatalysis; surface area; titania

DOI: 10.14359/51686985

Date: 3/1/2015

Abstract:
While there is an increasing interest in using photocatalytic cement-based materials, a lack of an appropriate standard procedure for testing the photocatalytic activity and efficiency of such materials makes comparisons among materials and data from different sources challenging. Current standard test methods are not appropriate for assessing photocatalytic nitrogen oxide conversion by cementitious materials because the standards do not consider surface properties of cementitious materials, nor are the test conditions appropriate for evaluation of cementitious materials. Therefore, the main objective is to propose a standard procedure for assessing the photocatalytic activity of cement mixtures with TiO2 additives and to define a parameter—the photocatalytic efficiency factor (PEF)—that could be used to compare the photocatalytic activity of different TiO2 cement mixtures, even for extended exposure conditions. The use of PEF is demonstrated, and values of PEF ranging from 8.40 to 51.55 μmol·h–1·m–2 (0.78 to 4.79 μmol·h–1·ft–2) was observed for mixtures with TiO2 up to 15% replacement.