Behavior of Fire-Damaged Mortar under Variable Re-curing Conditions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Fire-Damaged Mortar under Variable Re-curing Conditions

Author(s): Michael Henry, Masamitsu Suzuki, and Yoshitaka Kato

Publication: Materials Journal

Volume: 108

Issue: 3

Appears on pages(s): 281-289

Keywords: carbonation; chemical analysis; crack self-healing; durability; fire damage; fire repair; re-curing; rehydration

DOI: 10.14359/51682493

Date: 5/1/2011

Abstract:
An experimental investigation on the effect of post-fire cooling and re-curing conditions on strength and durability of normal- and high-strength cement mortars was conducted. Results showed that air re-curing resulted in the formation of surface cracks due to differential thermal shrinkage, which reduced the strength. An increase in air permeability indicated low durability; carbonation also occurred in these specimens. Immediate water submersion resulted in large strength reduction, but was followed by strength, porosity, and crack recovery due to rehydration, which also prevented carbonation. Specimens that cooled in the air before being submerged in water lost less strength but also recovered less quickly. A chemical analysis of the high-strength specimens found that growth in the pore structure could be attributed to the rehydration of hydration products that were dehydrated during heating. Complete strength recovery, however, was not observed, which may be attributed to the instability of self-healed cracks.