Title: 325.10R-95: Report on Roller-Compacted Concrete Pavements (Reapproved 2001)

Author(s): ACI Committee 325

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 32

Keywords: pavements

Date: 3/1/1995

Abstract:
This report covers the present state of the art for roller-compacted concrete pavements. It contains information on applications, material properties, mix proportioning, design, construction, and quality control procedures. Roller-compacted concrete use for pavements is relatively recent and the technology is still evolving. The pavement consists of a relatively stiff mixture of aggregate, cementitious materials and water, that is compacted by rollers and hardened into concrete.




  

Please enter this 5 digit unlock code on the web page.