Title: 301-96: Specifications for Structural Concrete for Buildings
Author(s):
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s): 43
Keywords: specifications
Date: 1/1/1996
Abstract:
Note: A newer version of this document exists. This document was replaced by 301-99.
Covers materials and proportioning of concrete; reinforcing and prestressing steels; production, placing, and curing of concrete; and formwork design and construction. Methods of treatment of joints and embedded items, repair of surface defects and finishing of formed surfaces are specified. Separate chapters include slab construction and finishing, architectural concrete, massive concrete, and materials and methods of construction, post-tensioned concrete. Provisions governing testing, evaluation, and acceptance of concrete as well as acceptance of the structure are included.