Abstract:

Note: A newer version of this document exists. This document was replaced by 225R-99.

Summarizes information about the composition and availability of commercial hydraulic cements and factors affecting their performance in concrete. The influences of admixtures (both chemical and mineral) and the environment on cement performance are discussed. Also covers the influence of cement on the properties of concrete.