International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design of Slender Columns Revisited

Author(s): J. G. Macgregor

Publication: Structural Journal

Volume: 90

Issue: 3

Appears on pages(s): 302-309

Keywords: columns (supports); frames; reinforced concrete; stability; structural design; phi; Design

DOI: 10.14359/4237

Date: 5/1/1993

Abstract:
Revisions are proposed to Sections 10.10 and 10.11 of the ACI Building Code to simplify the design of slender columns and to recognize the use of second-order analyses. These changes are undergoing letter ballot in ACI Committee 318 and if accepted will appear in the 1995 ACI Code. Major changes include the listing of a series of EI values for use in second-order frame analyses, a test for sway and nonsway frames, a flat value for stability calculations, new slenderness limits, and the method of combining and magnifying the nonsway and sway moments.


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer