Title: Compressive Strength and the Rising Temperature of Field Concrete

Author(s): Martin Mittelacher

Publication: Concrete International

Volume: 14

Issue: 12

Appears on pages(s): 29-33

Keywords: admixtures; portland cement compound composition; concrete mixes; compressive strength; concretes; field tests; set retarding agents; slump tests; statistical analysis; temperature; Structural Research

DOI:

Date: 12/1/1992

Abstract:
Over 2500 concrete test reports from 14 Florida and Georgia projects were evaluated for the correlation between increases in placing temperatures and compressive strengths. The 22 data sets in this review represented mixtures of design strengths between 3000 and 10,000 psi. Placing temperatures varied between 48 F and 100 F.




  