Title: Corrosion Inhibitors in Concrete

Author(s): Neal S. Berke

Publication: Concrete International

Volume: 13

Issue: 7

Appears on pages(s): 24-27

Keywords: chlorides; corrosion; corrosion resistance; permeability; reinforced concrete; spalling; General

Date: 7/1/1991

Abstract:
One means of protecting reinforcing steel from corrosion is to add an inhibitor to the concrete. In this paper, a review of the use of corrosion inhibitors in concrete is presented and with a focus on calcium nitrate.