Rehabilitation Strategies

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Rehabilitation Strategies

Author(s): Robert G. Tracy and Russel S. Fling

Publication: Concrete International

Volume: 11

Issue: 9

Appears on pages(s): 41-45

Keywords: classifying; concretes; damage; deterioration; reinforced concrete; renovating; repairs; reviews; General

DOI:

Date: 9/1/1989

Abstract:
While there is much written information available to the rehabilitation engineer in the form of ACI committee reports, codes, and specifications as well as other technical reports, such information is not wholly focused on restoration program development. This article should assist restoration professionals, various technical committees, and other interested parties in pinpointing the areas in which they can expedite development of effective programs and publishing information relating to rehabilitation.