Structural System Performance in Parking Structures

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Structural System Performance in Parking Structures

Author(s): Anthony P. Chrest

Publication: Concrete International

Volume: 12

Issue: 8

Appears on pages(s): 30-34

Keywords: concrete durability; concrete slabs; corrosion resistance; cracking (fracturing); deicers; parking facilities; performance; post-tensioning; precast concrete; reinforced concrete; General

Date: 8/1/1990

Abstract:
Compares the suitability of various structural systems for parking structures in corrosive environments. Describes the structural systems discussed and examines the factors that would tend to make them more or less vulnerable to environmental attack in places where road salt is used in the winter and in areas near the sea. 604-590