Title: Determining Tensile Properties of Mass Concrete by Direct Tensile Test

Author(s): Xie Nianxiang and Liu Wenyan

Publication: Materials Journal

Volume: 86

Issue: 3

Appears on pages(s): 214-219

Keywords: aggregate size; mass concrete; modulus of elasticity; specimens; strains; tensile strength; tension tests; Materials Research

DOI: 10.14359/2397

Date: 5/1/1989

Abstract:
Strength, strain capacity, and modulus of elasticity were determined for eighty large prism specimens with enlarged ends, 45 x 45 cm in cross section and 360 cm long, and eighty 10 x 10 x 55 cm small prism specimens. The relationships between the tensile properties of full-mix mass concrete with 150 mm maximum size aggregate (MSA) and that of the same concrete wet-screened to 40 mm MSA and tested in small specimens were obtained. The relationship of tensile properties of the same concrete tested in large and small specimens also were studied.