Title: Concrete Over the Top--Or, is there Life After Peak?

Author(s): Shawn S. Smith, Kasper J. Willam , Kurt H. Gerstle, and Stein Sture

Publication: Materials Journal

Volume: 86

Issue: 5

Appears on pages(s): 491-497

Keywords: brittleness; compressive strength; concretes; ductility; strain hardening; strains; tests; triaxial stresses; Materials Research

DOI: 10.14359/2089

Date: 9/1/1989

Abstract:
Test results are presented showing the post-peak response of concretes of three different strengths under triaxial stress states. These test results clearly show the transition from brittle to ductile behavior under increasing confinement, the residual strength, and the strain behavior at and after peak. Some evidence is also presented that indicates that Drucker's postulate may be relaxed for concrete. Concretes of different strengths behave similarly, with increasing brittleness for higher strength concretes.