Concrete Q & A: Selecting Repair Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Q & A: Selecting Repair Materials

Author(s):

Publication: Concrete International

Volume: 29

Issue: 4

Appears on pages(s): 115-116

Keywords:

DOI:

Date: 4/1/2007

Abstract:
1. I have a crack in a foundation wall that starts from the corner of a rectangular penetration and runs almost vertically down the height of the wall. After a heavy rain, water leaks into the foundation through the crack. When contacted about needed repairs, one contractor recommended injecting epoxy into the crack, and another recommended injecting polyurethane. Which one will give the best repair? 2. We have to repair some thin delaminations on a concrete slab. What types of products work best for this application?