Title: Another Look at Cracking and Crack Control in Reinforced Concrete

Author(s): Frosch, R. J.

Publication: 318Reference

Volume: 10

Issue: 16

Appears on pages(s): pp. 437-442

Keywords:

Date: 6/1/2005

Abstract:
ACI Structural Journal, V. 96, No. 3, May-June 1999