Abstract:
Results of a laboratory study of no-fines pervious concrete for paving are presented. Conclusions are drawn regarding the percentage of air voids needed for adequate permeability, the optimum water-cement ratio range, and the amounts of compaction and curing required. Recommendations are made regarding appropriate uses for this type of concrete.




  