Title: Post-Tensioning With Thread-Bars
Author(s): Richard Heinen
Publication: Symposium Paper
Volume: 26
Issue:
Appears on pages(s): 741-751
Keywords: anchorage (structural); bond (concrete to reinforcement); corrosion resistance; post-tensioning; prestressed concrete; prestressing steels; stress corrosion
Date: 1/1/1971
Abstract:
The paper reports on new prestressing tendons, which have been designed to achieve reliable bond, to guarantee corrosion protection, and to eliminate elastic and plastic slippage in anchors and couplings. Information about comparative tests on stress corrosion will be given.