Title: Fatigue Characteristics of Welded Wire Fabric

Author(s): N.M. Hawkins and L.W. Heaton

Publication: Special Publication

Volume: 41

Issue:

Appears on pages(s): 183-202

Keywords: bending; cracking (fracturing); deformations (reinforcing steels); fatigue (materials); fatigue tests; reinforcing; steels; static tests; stresses; welded wire fabric

Date: 1/1/1974

Abstract:
Results are reported of tests to determine the factors dictating the short life fatigue characteristics in air of a square smooth welded wire fabric consisting of No. 2 wires at 6 inch (15 cm) centers.