Computer-Aided Limit State Design for Reinforced Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Computer-Aided Limit State Design for Reinforced Concrete Structures

Author(s): V. Ramakrishnan

Publication: Symposium Paper

Volume: 33

Issue:

Appears on pages(s): 239-258

Keywords: bridges (structures); computer programs; continuous beams; elastic analysis; frames; limit design method; limit state design; loads (forces); moments; multistory buildings; reinforced concrete; statically inderminate strucures; structural analysis

DOI: 10.14359/17664

Date: 1/1/1972

Abstract:
Presents general computer programs for determining the ultimate load for any type of reinforced concrete indeterminate structure by using the limit state design procedure suggested by Baker.




  