Title: How to Design for Torsion

Author(s): Alan H. Mattock

Publication: Symposium Paper

Volume: 18

Issue:

Appears on pages(s): 469-495

Keywords:

Date: 1/1/1968

Abstract:
The need to take torsion into account explicitly in design is discussed in the light of refinement of flexural design and reduction of factors of safety. Behavior in pure torsion is considered, and the interaction between torsion, shear and flexural strengths is discussed.




  