Dynamic Torsion of Plain Concrete Elements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Dynamic Torsion of Plain Concrete Elements

Author(s): Rudolph Szilard

Publication: Symposium Paper

Volume: 18

Issue:

Appears on pages(s): 239-260

Keywords:

DOI: 10.14359/17571

Date: 1/1/1968

Abstract:
The paper describes an experimental and analytical investigation of the dynamic behavior of plain concrete elements, of circular and square cross-sections, subjected to rapidly applied torques.




  