Title: Behavior of Concrete Members Subject to Torsion and to Combined Torsion, Bending, and Shear

Author(s): E.L. Kemp

Publication: Symposium Paper

Volume: 18

Issue:

Appears on pages(s): 179-202

Keywords:

Date: 1/1/1968

Abstract:
Discussion proceeds from the simplest case of pure torsion for members without web reinforcement to the complex case of combined torsion, bending and shear.




  