Title: Classification of Fasteners for Concrete

Author(s): Ben L. Bird

Publication: Symposium Paper

Volume: 22

Issue:

Appears on pages(s): 31-44

Keywords: anchoring; anchors; bolts; concrete blocks; concretes; costs; drilling; expansion bolts; fasteners; inserts; lag bolts; loads (forces); nails; precast concrete; screws; studs; toggle bolts

Date: 1/1/1969

Abstract:
There are six general considerations for fasteners: (1) load level, weight held; (2) load condition-dead, variable, vibratory, shock; (3) base material; (4) atmospheric condition; (5) in-place cost and (6) simplicity of design.




  