Title: Biaxial Bending Simplified

Author(s): Albert J. Gouwens

Publication: Special Publication

Volume: 50

Issue:

Appears on pages(s): 233-263

Keywords: axial loads; bending; biaxial loads; columns (supports); loads (forces); moment distribution; moments; reinforced concrete; reinforcing steels; stress-strain relationships; structural analysis; structural design

Date: 1/1/1975

Abstract:
A comprehensive but simple design procedure is presented for the design of concrete columns subject to biaxial bending. The procedure is oriented towards hand computation but is suitable for incorporation into computer programs. The methods in the existing literature are summarized and evaluated. A new design procedure and an example problem showing its use are given.