Title: Bent-Up Bars as Shear Reinforcement

Author(s): P.E. Regan and M.H. Khan

Publication: Symposium Paper

Volume: 42

Issue:

Appears on pages(s): 249-266

Keywords: bars; beams (supports); bent-up bars; crack width and spacing; cracking (fracturing); reinforced concrete; reinforcing concrete; reinforcing steels; shear strength; tests

Date: 1/1/1974

Abstract:
The paper describes the results of a series of tests of beams reinforced with bent-up bars.




  