Title: Model Studies on a Beam-and-Slab Concrete Bridge under Concentrated Loadings

Author(s): L.K. Stevens and K.B. Gosbell

Publication: Symposium Paper

Volume: 23

Issue:

Appears on pages(s): 55-74

Keywords: aircraft; beams (structural); bending moments; bridge decks; bridges (structures); composite construction (concrete to concrete); deflection; diaphragms (concrete); load transfer; loads (forces); models; moving loads; precast concrete

Date: 1/1/1969

Abstract:
The deck of a tunnel under an airport runway is subjected to large concentrated loads, which make it imperative that design methods be checked experiementally to verify distribution of loads, stresses and deflections.




  