Title: A Testing Agency's Experience With Expansive Cements

Author(s): Edward H. Rubin

Publication: Symposium Paper

Volume: 38

Issue:

Appears on pages(s): 341-352

Keywords: admixtures; compressive strength; concrete construction; drying shrinkage; expansive cement concretes; expansive cements; high temperature; hydration; lightweight aggregate concrete; mix proportioning; research; shrinkage-compensating cements; slump tests

DOI: 10.14359/17211

Date: 1/1/1973

Abstract:
An independent commercial testing agency has over the past years accumlated considerable experience in working with expansive cements of the shrinkage-compensating type.




  