Title: Design of Shrinkage-Compensating Concrete Slabs

Author(s): Henry G. Russell

Publication: Symposium Paper

Volume: 38

Issue:

Appears on pages(s): 193-226

Keywords: concrete slabs; cracking (fracturing); drying shrinkage; expansive cement type K; expansive cement type M; expansive cement type S; expansive cements; lightweight concretes; reinforced concrete; restraints; shrinkage compensating concretes; strains

Date: 1/1/1973

Abstract:
Initial results are reported from a laboratory investifation to determine time-dependent properties of reinforced concrete slabs made wuth shrinkage-compensating concretes.




  