207.1R-87: Mass Concrete
Author(s):
Publication:
Technical Documents
Volume:
Issue:
Appears on pages(s):
44
Keywords:
admixtures; aggregate gradation; aggregate size; aggregates; air entrainment; arch dams; batching; bridge piers; cements; compacting; compressive strength; concrete construction; concrete dams; concrete durability; cooling; cracking (fracturing); creep pr
DOI:
Date:
11/21/1996
Abstract:
Note: A newer version of this document exists. This document was replaced by 207.1R-96.
Report presents a discussion of materials and practices employed in proportioning, mixing, placing, and curing mass concrete. Particular emphasis is placed on the difference between mass concrete and other concrete. The report is designed to serve as a re