Title: Fatigue Tests of Pretensioned Girders with Blanketed and Draped Strands

Author(s): Rabbat, B. G.; Kaar, P. H.; Russell, H. G.; and Bruce, R. N., Jr.

Publication: 318Reference

Volume: 12

Issue: 27

Appears on pages(s): pp. 88-114.

Keywords:

Date: 6/1/2008

Abstract:
Journal of the Prestressed Concrete Institute, V. 24, No. 4, July-Aug. 1979




  