Title: Prestressed Concrete Tank Performance

Author(s): Morris Schupack

Publication: Symposium Paper

Volume: 8

Issue:

Appears on pages(s): 55-65

Keywords:

Date: 1/1/1964

Abstract:
The behavior of prestressing wire in both sewage and water storage tanks is described. The conditions which led to the failure of a sludge digestion tank and the opinions of the cause of failure are discussed, and methods of avoiding problems suggested.




  