Title: Fire Resistance of Reinforced Concrete

Author(s): I. A. Benjamin

Publication: Symposium Paper

Volume: 5

Issue:

Appears on pages(s): 25-39

Keywords:

Date: 1/1/1962

Abstract:
Examines the effect of thermal and structural factors on the fire endurance of normal reinforced concrete. The effects on fire endurance of such variables as type of aggregate, moisture content of the specimen, and the ability of cover to remain in place are discussed.




  