Title: 
            Flexural Behavior of High-Strength Concrete Beams
        
        
            Author(s): 
            Leslie, K. E.; Rajagopalan, K. S.; and Everard, N. J.
        
        
            
                Publication: 
                Commentary Reference
            
            
                Volume: 
                10
            
            
                Issue: 
                1
            
            
                Appears on pages(s): 
                pp. 517-521.
            
            
                Keywords: 
                
            
            
                DOI: 
                
            
        
        
            Date: 
            6/1/2008
        
        
            Abstract:
            ACI JOURNAL, Proceedings V. 73, No. 9, Sept. 1976