Title: Progress In the Use of Metal Forms with Comparative Costs

Author(s): W.L. Caldwell

Publication: Journal Proceedings

Volume: 5

Issue: 1

Appears on pages(s): 347-354

Keywords: none

Date: 1/1/1909

Abstract:
Owing to the falling off in building operations during the past year, there has not been as much interest shown in the development of the metal forms as otherwise would have been, consequently there has not been the opportunity to develop this method to the extent anticipated. However, we have given the subject considerable thought and believe have materially improved on the suggestions submitted a year ago at the Convention in Buffalo.




  