Title: Measuring Consistency of Freshly Mixed Concrete

Author(s): Guo Chengju

Publication: Concrete International

Volume: 9

Issue: 8

Appears on pages(s): 62-67

Keywords: compacting; consistency tests; fresh concretes; vibration; mix proportioning; no-slump concrete; roller-compacted concrete; quality control; workability; Materials Research

DOI:

Date: 8/1/1987

Abstract:
A simple yet useful method of measuring the consistency of freshly mixed concretes, ranging from wet to very dry, is discussed. The consistency of concrete is represented by the compacting factor measured when a definite amount of work is done on a sample




  