Title: Proposed Standard Specifications for Concrete Drain Pipe and Tile
Author(s): ACI Committee on Specifications for Concrete Drain Pipe and Tile
Publication: Journal Proceedings
Volume: 7
Issue: 12
Appears on pages(s): 761-765
Keywords: none
Date: 12/1/1911
Abstract:
The cement shall meet the requirements of the Standard Specifications for Portland Cement of the American Society for Testing Materials and adopted by this Association. (Standard No. 1.) This paper includes materials, proportions, mixing, forming, curing, dimensions, and finished title.