In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
American Concrete Institute 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA
Phone: 1.248.848.3700 Fax: 1.248.848.3701 Staff Directory
Chat with Us Online Now
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: The Present Status of Unit Concrete Construction
Author(s): James L. Darnell
Publication: Journal Proceedings
Volume: 8
Issue: 3
Appears on pages(s): 455-468
Keywords: none
Date: 3/1/1912
Abstract:To put it briefly it might be said that the present status of Unit Construction is one of progression. Every day new things are developing about this very logical and rational method of constructing and erecting concrete structures. Within the past two years there has been more progress in both the design and in the field work, that is, the construction and erection of separately molded structures, than in all the time previous.