Appendix to Report of Committee on Research, American Concrete Institute, 1922

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Appendix to Report of Committee on Research, American Concrete Institute, 1922

Author(s): ACI Committee E-3

Publication: Journal Proceedings

Volume: 18

Issue: 2

Appears on pages(s): 206-216

Keywords: none

DOI: 10.14359/15686

Date: 2/1/1922

Abstract:
Investigations in concrete carried on by the University of Minnesota are being conducted by Professors Maney and M.B. Lagaard in the structural division of the civil department, and by Prof. F.C. Lang, of the highway division. The major part of the work, begun by Mr. MacMillian, is still being carried on at the university. There were also a series of tests.




  