Title: Standard Specifications for Portland Cement Concrete Sidewalks

Author(s): ACI Committee C-2

Publication: Journal Proceedings

Volume: 21

Issue: 2

Appears on pages(s): 591-596

Keywords: none

Date: 2/1/1925

Abstract:
These specifications cover both one- and two-course sidewalk construction. The specifications for materials and construction included in Paragraphs 1 to 36 inclusive, apply to both one- and two-course types of sidewalks.




  