Title: Building Fireproof Homes
Author(s): Paul Hueber
Publication: Journal Proceedings
Volume: 20
Issue: 2
Appears on pages(s): 487-494
Keywords: none
DOI: 10.14359/15507
Date: 2/1/1924
Abstract: Fireproof homes are by means a new product. Well-to-do men have been building such homes for years, not because they wanted a cheaper house, but because they wanted the best. These were built according to architects’ designs and special forms were required for each house.