Title: A Demonstration in Making Trim Stone and Ornamental Concrete
Author(s): R.F. Havlik
Publication: Journal Proceedings
Volume: 20
Issue: 2
Appears on pages(s): 250-258
Keywords: none
Date: 2/1/1924
Abstract:
At Mooseheart we manufacture trimstone and building block for our own and for a few customers such as Marshall Field & Co. and Wanamaker, and about two other concerns like that in the larger cities. The reason we manufacture garden furniture is to give the boys experience in making ornamental products. It is impossible to put enough ornaments into an ordinary building to give the boys sufficient practice in such work.