Title: Making Good Concrete
Author(s): Duff A. Abrams
Publication: Journal Proceedings
Volume: 20
Issue: 2
Appears on pages(s): 175-181
Keywords: none
Date: 2/1/1924
Abstract:
The type and adaptation of structural materials is one of the best criteria of the development of the race. Reinforced-concrete is the newest arrival in the long list of materials which have been used by man for shelter, protection, convenience, or ornament.