The Architectural Uses of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Architectural Uses of Concrete

Author(s): Irving K. Pond

Publication: Journal Proceedings

Volume: 23

Issue: 2

Appears on pages(s): 269-273

Keywords: none

DOI: 10.14359/15416

Date: 2/1/1927

Abstract:
Some few years ago, as chairman of a committee of the American Institute of Architects, I submitted a report on the uses of concrete in architecture which met with favor and was published separately by the Institute and widely distributed. I refer to that report as it was responsible for my giving a paper along lines suggested therein before a convention of this organization shortly after its appearance. I have only a vague recollection at this time of what was contained in either the report or the paper; only a detail here and there of either standing out in my memory.




  

Edit Module Settings to define Page Content Reviewer